01. Blow Molding Machine Operation Procedures

  1. Study Manual First: Before familiarizing yourself with the machine’s performance and operation sequence, read the manual thoroughly to understand its capabilities and procedures. Only operate after complete familiarity.
  2. Check Hydraulic Oil Level: Before starting, ensure hydraulic oil reaches at least 2/3 of the level gauge indicator. If not, add the same type of hydraulic oil.
  3. Lubrication System Check: Verify the manual oil pump has sufficient lubricant. If empty, fill with the same type of lubricating oil to within scale range. Pump the handle until lubricant appears at all lubrication points.
  4. Safety Guard Requirement: Do not operate if guards are missing or equipment is malfunctioning.
  5. Door Safety Interlock: Never start the machine with doors open.
  6. Clear Obstructions: Remove all foreign objects, especially from moving parts, before operation.
  7. Cooling Water Pressure: Maintain water pressure between 2-6 kgf/cm².
  8. Pre-Start Inspection: Check for electrical shorts/leakage, open oil circuit sections, and ensure no personnel are working on the frame. Resolve any issues before operation.
  9. Heating Procedure: Preheat the barrel and head until reaching set temperature, then maintain for at least 5 minutes before starting.
  10. Air Pressure Setup: Start air pressure pump to achieve 5-8 kgf/cm² before operation.
  11. Single Operator Rule: Only one operator permitted except during mold installation. Ensure no personnel in hazardous areas before activation. Test operations by pressing start button and observe normal operation before releasing.
  12. Parameter Setting: Set operating parameters according to the “Process Card.” Check critical processes every two hours and record in production monitoring log.
  13. Emergency Response: Stop immediately if malfunctions occur and notify maintenance personnel.
  14. Safety Zone Protocol: No personnel allowed inside doors or protective barriers during operation.
  15. Pressure Monitoring: System pressure must not exceed 140 kgf/cm², normal operating pressure should stay below 100 kgf/cm². Accumulator pressure must not exceed set value. Verify heating system temperature within set range (±10℃ tolerance).
  16. Shutdown Procedure: Switch to manual mode, return to origin position, turn off oil pump and heating switches, then cut main power.

02. Common Blow Molding Issues and Solutions

01 Poor PET Bottle Transparency

  • Causes:
    1. Excessive heating temperature/duration
    2. Moisture in compressed air
    3. Opaque preform material
    4. Improper preform design
    5. Insufficient blow ratio
  • Solutions:
    1. Reduce temperature/shorten heating time
    2. Install air dryer
    3. Improve preform quality with better materials and drying
    4. Optimize preform dimensions
    5. Reduce preform diameter

02 Uneven Wall Thickness

  • Causes:
    1. Misaligned stretch rod
    2. Asymmetric/irregular air vents
    3. Low stretch ratio/blow ratio
    4. Non-rotating preforms in heater
    5. Uneven preform wall thickness/injection density
  • Solutions:
    1. Adjust stretch rod position and air vents
    2. Increase stretch/blow ratio
    3. Check rotation mechanism and improve preform quality

03 Thin Bottle Bottom

  • Causes:
    1. Premature blowing start
    2. Excessive bottom temperature
    3. Thin preform bottom
  • Solutions:
    1. Delay blowing start time
    2. Reduce bottom temperature
    3. Increase preform bottom thickness

04 Visible Mold Parting Line

  • Causes:
    1. Insufficient mold clamping pressure
    2. Early sealing time
    3. Mold-preform thread size mismatch
  • Solutions:
    1. Increase clamping pressure, adjust support rod angle (<5°)
    2. Reposition mold travel switch
    3. Repair mold/check assembly (guide pins, fastening)
    4. Maintain mold thread engagement

05 Curling/Accumulation at Bottom/Neck

  • Causes:
    1. Overlong blowing time
    2. Inconsistent curling
    3. Low temperature at accumulation points
    4. Unstable air pressure affecting stretch rod speed
  • Solutions:
    1. Shorten blowing time/reduce stretch rod speed
    2. Reduce air volume on curling side
    3. Increase local heating temperature
    4. Add air reservoir/shorten air supply lines

06 Deformed Bottom

  • Causes:
    1. Slow stretch rod speed
    2. Insufficient blowing time
    3. Severe preform eccentricity
  • Solutions:
    1. Maximize throttle valve on stretch cylinder
    2. Extend blowing time
    3. Measure preform eccentricity (bending occurs with high eccentricity at elevated temperatures)
    4. Include temperature protection measures

This comprehensive guide ensures safe operation and effective troubleshooting for optimal blow molding performance. Always prioritize safety and regular maintenance for sustained equipment efficiency.

About Figo Hussain

I’m Figo Hussain, founder of FAYGO UNION, with 20 years of experience providing innovative plastic machinery solutions worldwide.

Talk With Author >>

Start Your Business With Us

Simple Contact Form

Contact Now-Faygo

Get The Quote

Contact Form

Contact Now-Faygo CEO

Get The Quote

Contact Form

Contact Now-Faygo

Get The Quote

Simple Contact Form